Thin films (100-1000 Å) of vanadium dioxide (VO2) were created by atomic-layer deposition (ALD) on sapphire substrates. Following this, the optical properties were characterized through the metal-insulator transition of VO2. From the measured optical properties, a model was created to describe the tunable refractive index of VO2.

Explore More Videos

Vanadium Dioxide Films

Chapters in this video

0:04

Title

0:56

Atomic Layer Deposition (ALD) of Amorphous Vanadium Dioxide (VO2 ) on Sapphire Substrates

3:06

Annealing Amorphous VO2 Thin Films

4:45

Characterization of VO2 Films by Raman Spectroscopy

5:43

Characterization of VO2 Films by X-Ray Photoelectron Spectroscopy (XPS)

7:31

Morphological Characterization by Atomic Force Microscopy (AFM)

9:06

Results: Characterization of Amorphousand Crystalline VO2 Films

10:49