Cell Nanoindentation

Cell nanoindentation is a mechanical characterization technique that measures how individual cells deform under a controlled, nanoscale force, revealing properties such as stiffness and viscoelasticity. Typically, an atomic force microscope or related instrument presses a calibrated probe into the cell while recording force and indentation depth; mathematical models convert these force-displacement measurements into quantitative mechanical parameters. In bioengineering, cell nanoindentation helps compare healthy and diseased cells, assess responses to drugs or substrate conditions, and characterize changes during differentiation, migration, and tissue development. These measurements connect cellular mechanics with structure, function, and disease-related phenotypes.

Cell Nanoindentation - Related Videos

Research

JoVE Journal - Bioengineering

Experimental and Data Analysis Workflow for Soft Matter Nanoindentation

0 Views •

Cited by 19 •

2022

The protocol presents a complete workflow for soft material nanoindentation experiments, including hydrogels and cells. First, the experimental steps to acquire force spectroscopy data are detailed; then, the analysis of such data is detailed through a newly developed open-source Python software, which is free to download from GitHub.

Atomic Force Microscopy Cantilever-Based Nanoindentation: Mechanical Property Measurements at the Nanoscale in Air and Fluid

0 Views •

Cited by 11 •

2022

Quantifying the contact area and force applied by an atomic force microscope (AFM) probe tip to a sample surface enables nanoscale mechanical property determination. Best practices to implement AFM cantilever-based nanoindentation in air or fluid on soft and hard samples to measure elastic modulus or other nanomechanical properties are discussed.

Research

JoVE Journal - Bioengineering
Free Sample

Characterization Of Multi-layered Fish Scales (Atractosteus spatula) Using Nanoindentation, X-ray CT, FTIR, and SEM

0 Views •

Cited by 15 •

2014

This paper presents the methods used for probing spatially correlated chemical, structural, and mechanical properties of the multilayered scale of Atractosteus spatula (A. spatula) using nanoindentation, Fourier transform infrared (FTIR) spectroscopy, scanning electron microscopy (SEM), and X-ray computed tomography (X-ray CT). The experimental results have been used to investigate the design principles of protective biological materials.

A Virtual Simulation Experiment of Mechanics: Material Deformation and Failure Based on Scanning Electron Microscopy

0 Views •

2023

This work presents a three-dimensional virtual simulation experiment for material deformation and failure that provides visualized experimental processes. Through a set of experiments, users can become familiar with the equipment and learn the operations in an immersive and interactive learning environment.

Impact Indentation for Assessing the Mechanical Properties of a Mouse Brain Tissue

0 Views •

2025

Source: Canovic, E. P., et. al., Characterizing Multiscale Mechanical Properties of Brain Tissue Using Atomic Force Microscopy, Impact Indentation, and Rheometry. J. Vis. Exp. (2016)The video demonstrates using impact indentation to measure the mechanical properties of a hydrated mouse brain tissue, including stiffness, energy dissipation, and damping, through probe displacement and velocity analysis.